SEM (Tescan Vega (LMU)) was utilized to observe the cross-sectional and surface area morphology of the membranes of different NP loadings (Figure 1 and Figure S1). Membranes were being damaged in liquid nitrogen to repair the cross-sectional ends from the membranes and also a voltage of fifteen–twenty Kv at different magnifications was applied wi